The invention discloses a new processing method for warm-keeping fabrics, which includes the following steps: step 1, cutting; step 2, setting; step 3, step 4; step 5, soft finishing; step 6, setting and drying, arranging the soaked Plush on the setting machine for setting, the setting temperature is 85 90 C, and setting. The drying time is 16 20 minutes, and the fluff after setting is arranged in the oven for drying at 125 130 C and 8 11 minutes. The process is simple and the operation method is simple. The products produced have the characteristics of good softness and warmth retention, good hand feeling and high comfort. It meets the market demand and is conducive to the promotion of products.
【技术实现步骤摘要】
一种保暖的新型面料的加工方法
本专利技术属于布的处理
,具体涉及一种保暖的新型面料的加工方法。
技术介绍
现有的毛绒布,存在以下不足:柔软性与保暖性差,毛绒布手感差,舒适度低,影响其使用。
技术实现思路
本专利技术的目的是提出一种保暖的新型面料的加工方法,其工艺简单,操作方法,生产的产品即具有柔软性与保暖性好的特点,还具有手感好、舒适度高的特点,满足市场使用需求,有利于产品的推广。为了达到上述设计目的,本专利技术采用的技术方案如下:一种保暖的新型面料的加工方法,包括以下步骤:步骤一、裁切,将坯布裁切为规格面料。步骤二、定型,将坯布织造成型的面料定型。步骤三、拉毛,将定型后的面料拉毛。步骤四、染色,将预定型后的绒类面料染色。步骤五、柔软整理,向染色后的面料加入浸泡液。步骤六、定型、烘干,将浸泡后的毛绒布置于定型机上进行定型,定型温度为85-90℃,定型时间为16-20分钟;定型后的毛绒布置于烘箱中干燥,干燥温度为125-130℃,干燥时间为8-11分钟。本专利技术具有柔软性与保暖性好的特点,还具有手感好、舒适度高的特点。具体实施方式下面结合具体实施例对本专利技术进一步阐释。一种保暖的新型面料的加工方法,包括以下步骤:步骤一、裁切,将坯布裁切为规格面料。步骤二、定型,将坯布织造成型的面料定型。步骤三、拉毛,将定型后的面料拉毛。步骤四、染色,将预定型后的绒类面料染色。步骤五、柔软整理,向染色后的面料加入浸泡液。步骤六、定型、烘干,将浸泡后的毛绒布置于定型机上进行定型,定型温度为85-90℃,定型时间为16-20分钟;定型后的毛绒布置于烘箱中干燥,干燥温度为12 ...
【技术保护点】
1.一种保暖的新型面料的加工方法,其特征在于,包括以下步骤:步骤一、裁切,将坯布裁切为规格面料;步骤二、定型,将坯布织造成型的面料定型;步骤三、拉毛,将定型后的面料拉毛;步骤四、染色,将预定型后的绒类面料染色;步骤五、柔软整理,向染色后的面料加入浸泡液;步骤六、定型、烘干,将浸泡后的毛绒布置于定型机上进行定型,定型温度为85‑90℃,定型时间为16‑20分钟;定型后的毛绒布置于烘箱中干燥,干燥温度为125‑130℃,干燥时间为8‑11分钟。
【技术特征摘要】
1.一种保暖的新型面料的加工方法,其特征在于,包括以下步骤:步骤一、裁切,将坯布裁切为规格面料;步骤二、定型,将坯布织造成型的面料定型;步骤三、拉毛,将定型后的面料拉毛;步骤四、染色,将预定型后的绒类面料染色;步骤五、柔软...