制造隔热砖的余料平铲制造技术

技术编号:18148803 阅读:72 留言:0更新日期:2018-06-09 01:27
本发明专利技术公开了一种制造隔热砖的余料平铲,一箱坯墩满箱后不能多也不能少,要得到更好地处理则要借助于本方案设计的余料平铲,余料平铲是根据普通铲改进的,余料铲与普通铲后部分不变,前部分改为铲口宽480毫米,铲口要平要直,铲口有刃,铲帮有一定的厚度,铲口的硬度和强度不要因受力而变型影响坯墩上一面的平度。

Spare shovel for making insulation bricks

The invention discloses a scraper for making heat insulation bricks. One box of billet piers can not be much or less after full box. To get better treatment, it is necessary to use the remainder shovel designed in this scheme. The spare shovel is improved according to the ordinary shovel. The spare shovel is changed from the common shovel, the front part is changed to the mouth width of 480 millimeters, shovel mouth. It must be straight and straight, the blade has a blade, and the shovel has a certain thickness. The hardness and strength of the shovel shall not affect the flatness of the side of the billet due to the deformation of the force.

【技术实现步骤摘要】
制造隔热砖的余料平铲
本专利技术是制造隔热砖的施工设备。
技术介绍
目前许多高层房屋建筑,为了不让地球的地壳承受太大的重量压力,都是采用各种各样的空心砖建筑墙体,这些建筑方式并没有给墙体减轻多大重量,不但重量没有减轻多少,其购买空心砖的成本也很高,无疑加重企业施工成本,带来经营风险,为此,研究专利技术适用的建筑施工方式和建筑材料投入高层房屋建筑施工,规避上述难以解决的困难,以提高施工生产效益,降低建筑成本是公众迫切需要解决的。
技术实现思路
本专利技术的目的在于提供一种能克服公知技术缺点,在一箱坯墩满箱后,依靠本专利技术使用方便,成本低廉的余料铲。为实现上述目的,本专利技术的方案为:一种制造隔热砖的余料铲,余料铲是根据普通铲改进的,余料铲后部分不变,前部分改为口宽480毫米,口平口直,铲口有刃,铲帮有一定的厚度。采用上述方案改变了以前落后方式,实现了本专利技术的目的。附图说明图1为制造隔热砖的余料平铲立体示意图。具体实施方式如图所示,在一箱坯墩满箱后不能多也不能少,要得到更好地处理则要借助于本方案设计的余料平铲,余料平铲是根据普通铲改进的,余料铲与普通铲后部分不变,前部分改为铲口宽480毫米,铲口要平要直,铲口有刃,铲帮有一定的厚度,铲口的硬度和强度不要因受力而变型影响坯墩上一面的平度。解决了已有脚疗技术缺陷,节约了大量的人力资源与物资资源。
制造隔热砖的余料平铲

【技术保护点】
一种制造隔热砖的余料平铲,其特征在于:一箱坯墩满箱后不能多也不能少,要得到更好地处理则要借助于本方案设计的余料平铲,余料平铲是根据普通铲改进的,余料铲与普通铲后部分不变,前部分改为铲口宽480毫米,铲口要平要直,铲口有刃,铲帮有一定的厚度,铲口的硬度和强度不要因受力而变型影响坯墩上一面的平度。

【技术特征摘要】
1.一种制造隔热砖的余料平铲,其特征在于:一箱坯墩满箱后不能多也不能少,要得到更好地处理则要借助于本方案设计的余料平铲,余料平铲是根据普通铲改进的,...

【专利技术属性】
技术研发人员:唐登巨
申请(专利权)人:岳池县福源创新科技有限公司
类型:发明
国别省市:四川,51

网友询问留言 已有0条评论
  • 还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。