The invention discloses a high performance nano composite material. The high performance nano composite material containing low density polyethylene 50 55% 5 9%; hydrotalcite; toughening agent 3.2 3.8% 12 29%; nano powder; antioxidant 0.8 stabilizer 3 4%; 10%; 10 wear-resisting agent 12%; the balance of deionized water. The advantages of the invention are: between each group of nano composite materials by a certain proportion and made good performance, high stability, nano powder and wear-resisting agent combined with each other, improve the wear resistance of the nano composite material, material properties of various materials by certain proportion and made stable. To strengthen the flexibility of composite material effectively, prolong the service life of composite materials.
【技术实现步骤摘要】
一种高性能纳米复合材料
本专利技术涉及到一种材料,尤其涉及到一种高性能纳米复合材料。
技术介绍
纳米复合材料一直是国内外材料科学研究领域的研究热点,通过运用现代纳米复合技术,可以对传统产业和产品进行性能上的更新和提高,不仅可以突破原有材料的基本性能,而且其他功能和功效上均有明显提高,而现有的纳米材料在柔韧性效果还欠佳,这样大大降低了产品的使用寿命。本专利技术涉及到的高性能纳米复合材料,其特征在于:所述高性能纳米复合材料包含低密度聚乙烯50-55%;水滑石5-9%;增韧剂3.2-3.8%;纳米粉体12-29%;抗氧剂0.8-10%;稳定剂3-4%;耐磨剂10-12%;余量为去离子水。材料中的各个组分之间通过一定的配比而制成,性能好,稳定性高,添加的纳米粉体和耐磨剂相互结合,提高了纳米复合材料的耐磨性能,各个原料之间通过一定的配比而成制成的板材性能稳定,能有效的加强复合材料的柔韧性,大大延长了复合材料的使用寿命。
技术实现思路
本专利技术解决其技术问题所采用的技术方案是一种高性能纳米复合材料,其特征在于:所述高性能纳米复合材料包含低密度聚乙烯50-55%;水滑石5-9%;增韧剂3.2-3.8%;纳米粉体12-29%;抗氧剂0.8-10%;稳定剂3-4%;耐磨剂10-12%;余量为去离子水。本专利技术的优点是:高性能纳米复合材料中的各个组分之间通过一定的配比而制成,性能好,稳定性高,添加的纳米粉体和耐磨剂相互结合,提高了纳米复合材料的耐磨性能,各个原料之间通过一定的配比而成制成的板材性能稳定,能有效的加强复合材料的柔韧性,大大延长了复合材料的使用寿命。具体实施方式具 ...
【技术保护点】
一种高性能纳米复合材料,其特征在于:所述高性能纳米复合材料包含低密度聚乙烯50‑55%;水滑石5‑9%;增韧剂3.2‑3.8%;纳米粉体12‑29%;抗氧剂0.8‑10%;稳定剂3‑4%;耐磨剂10‑12%;余量为去离子水。
【技术特征摘要】
1.一种高性能纳米复合材料,其特征在于:所述高性能纳米复合材料包含低密度聚乙烯50-55%;水滑石5-9%;增韧剂...