The invention discloses a building decorative plate made of cement, fly ash, fine sand, wood powder, terylene short fiber, viscose, the components by weight ratio: cement: Fly Ash: Sand: wood powder: terylene short fiber viscose =30:15:20:18:12:5; the material is placed in a blender, add appropriate amount of water after mixing, the rolling process. The invention has the advantages of no damage to human health, safety, non-toxic, tasteless, light texture, good strength and breathability, water absorption performance, fire resistance and moisture resistance, and can be used as ceilings or as decorative walls.
【技术实现步骤摘要】
本专利技术涉及建筑材料,特别是一种建筑装饰板材。
技术介绍
目前,建筑用装饰板材大多采用木质板、石膏板、石棉板、矿棉吸膏板等,其弊端是易烧、怕潮、易变形、有毒有污染,对人体健康有害。
技术实现思路
本专利技术的目的是针对传统技术存在的弊端,而提供一种建筑装饰板材,这种板材对人体健康无损害,重量轻,防水防潮不变形,同时又具有较好的强度和吸水透气性能。为实现上述技术目的,本专利技术采取的技术方案是:一种建筑装饰板材,由以下组份组成:水泥、粉煤灰、细砂、木粉、睛纶短绒、粘胶,各组分按重量份比例为:水泥:粉煤灰:细砂:木粉:睛纶短绒:粘胶=30:15:20:18:12:5;其生产方法为:按上述材料名称,根据各种原料的比例,选齐材料备用;将上述原料中的细砂用水淘洗干净备用,然后,将上述材料置于搅拌器内加适量的温水搅拌后,再经滚压成形而制得。本专利技术对人体健康安全无损,无毒无味,质地轻,具有较好的强度和透气、吸水性能,并能防火防潮,可用作天花板或作为墙的装饰。具体实施方式:下面结合实施例对本专利技术作进一步的说明一种建筑装饰板材,由水泥、粉煤灰、细砂、木粉、睛纶短绒、粘胶组成,各组分按重量份比例为:水泥:粉煤灰:细砂:木粉:睛纶短绒:粘胶=30:15:20:18:12:5;其生产方法为:按上述材料名称,根据各种原料的比例,选齐材料备用;将上述原料中的细砂用水淘洗干净备用,然后,将上述材料置于搅拌器内加适量的温水搅拌后,再经滚压成形而制得。本专利技术对人体健康安全无损,无毒无味,质地 ...
【技术保护点】
一种建筑装饰板材,其特征在于:所述板材由以下组份组成:水泥、粉煤灰、细砂 、木粉、睛纶短绒、粘胶,各组分按重量份比为:水泥:粉煤灰:细砂 :木粉:睛纶短绒:粘胶=30:15:20:18:12:5。
【技术特征摘要】
1.一种建筑装饰板材,其特征在于:所述板材由以下组份组成:水泥、粉煤灰、细砂、木粉、睛纶短绒、粘胶,各...
【专利技术属性】
技术研发人员:不公告发明人,
申请(专利权)人:哈尔滨鸿雁翔贸易有限公司,
类型:发明
国别省市:黑龙江;23
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。