The invention discloses a method for producing colored silk, relates to the technical field of textile products manufacturing; it includes the following steps: selecting cocoon, cocoon, cocoon, the cocoon baking, baking time 3 ~ 5 minutes, the cocoon bibulous rate reached more than 95%, the baked cocoon into the dye pool immersion dyeing, soaking temperature is 40 to 50 DEG C, the soaking time is 25 ~ 30 minutes after the dye cocoon into a container containing immersion fixing agent, soaking for 15 to 20 minutes, and then stripping cocoon, opening, dried, and pull Xu needle etc., are colored silk. Compared with the prior art, the present invention provides a method for producing colored silk quilt.
【技术实现步骤摘要】
有色蚕丝被的生产方法
本专利技术涉及家纺产品制造
,尤其是一种有色蚕丝被的生产方法。
技术介绍
蚕丝被因其柔软暖和,重量轻巧,冬暖夏凉,促进睡眠并且不易过敏,而受到广大消费者的喜爱,蚕丝被以蚕丝作为主要原料,在生产时需经过选茧、煮茧、剥茧、开棉、晒干、拉絮、定针等一系列工序,才能制作出品质上乘的蚕丝被,由于蚕丝中约97%的成分是纯天然动物蛋白,跟人体皮肤接近,因此蚕丝被大多为本色,无法满足现代人对视觉色彩的多种需要。
技术实现思路
本专利技术的目的是提供一种有色蚕丝被的生产方法。为了解决上述问题,本专利技术采用的技术方案是:一种有色蚕丝被的生产方法,包括选茧,煮茧,以及以下步骤:A、煮茧后,将蚕茧进行烘烤,烘烤时间3~5分钟,使蚕茧的吸水率达到95%以上;B、将步骤A烘烤后的蚕茧放入染料池浸泡染色,浸泡温度为40~50℃,浸泡时间为25~30分钟;C、将步骤B染色后的蚕茧放入含有固色剂的容器浸泡,浸泡时间为15~20分钟;D、将步骤C固色后的蚕茧进行剥茧、开棉、晒干、拉絮和定针等工序,得到有色蚕丝被。由于采用了上述技术方案,本专利技术与现有技术相比具有如下有益效果:1、在染色前对蚕茧进行烘烤,让蚕茧保持较高的吸水率,可以使蚕茧在染色时将染料吸收完全。2、染色后使用固色剂,使制成后的蚕丝被色牢度高。具体实施方式下面结合具体实施例对本专利技术作进一步详述:实施例1:一种有色蚕丝被的生产方法,包括选茧,煮茧,以及以下步骤:A、煮茧后,将蚕茧进行烘烤,烘烤时间3分钟,使蚕茧的吸水率达到95%以上;B、将步骤A烘烤后的蚕茧放入染料池浸泡染色,浸泡温度为40℃,浸泡 ...
【技术保护点】
一种有色蚕丝被的生产方法,包括选茧,煮茧,其特征在于还包括以下步骤:A、煮茧后,将蚕茧进行烘烤,烘烤时间3~5分钟,使蚕茧的吸水率达到95%以上;B、将步骤A烘烤后的蚕茧放入染料池浸泡染色,浸泡温度为40~50℃,浸泡时间为25~30分钟;C、将步骤B染色后的蚕茧放入含有固色剂的容器浸泡,浸泡时间为15~20分钟;D、将步骤C固色后的蚕茧进行剥茧、开棉、晒干、拉絮和定针等工序,得到有色蚕丝被。
【技术特征摘要】
1.一种有色蚕丝被的生产方法,包括选茧,煮茧,其特征在于还包括以下步骤:A、煮茧后,将蚕茧进行烘烤,烘烤时间3~5分钟,使蚕茧的吸水率达到95%以上;B、将步骤A烘烤后的蚕茧放入染料池浸泡染色,浸泡温...