The invention relates to a high gloss appearance of wool fabrics, including wool fiber and vinylon fiber, the wool fiber specifications for fineness of 85s ~ 150s and 95 ~ 115mm in length; the vinylon fiber size 3.5 ~ 4.5dtex * 50 ~ 75mm; which is characterized in that the wool fiber and vinylon fiber containing a good agent, the weight percentage of wool fiber and vinylon fiber: 68 ~ 85:76 ~ 92. The advantages compared with the prior art, which is: adding brightener in wool fiber and vinylon fiber, which makes the wool fabric high gloss, used clothing appearance made the wool fabric, feel smooth.
【技术实现步骤摘要】
本专利技术涉及纺织领域,特别涉及一种外表光泽度高的羊毛面料。
技术介绍
现有技术中有一种羊毛面料,包括羊毛纤维和维纶纤维,所述羊毛纤维的规格为细度85s~150s、长度95~115mm;所述维纶纤维的规格为3.5~4.5dtex×50~75mm。这种羊毛面料具有保暖、吸湿、富于弹性和耐磨的特点,但是这种羊毛面料光泽度低,表面暗淡,使用这种羊毛面条制成的成衣美观性差。
技术实现思路
针对上述缺点,本专利技术目的在于提供一种外表光泽度高的羊毛面料,表面光泽度高。为实现上述目的,本专利技术采用的技术方案是:一种外表光泽度高的羊毛面料,包括羊毛纤维和维纶纤维,所述羊毛纤维的规格为细度85s~150s、长度95~115mm;所述维纶纤维的规格为3.5~4.5dtex×50~75mm;其特征在于,羊毛纤维和维纶纤维内含有增光剂,所述羊毛纤维和维纶纤维的重量百分比为:68~85:76~92;所述增光剂包括以下重量百分比的组分:2-甲基-4-异噻唑啉-3-酮:17~32,2-正辛基-4-异噻唑啉-3-酮:17~32,丁二烯-苯乙烯乳液:8~15,纳米二氧化钛:8~15,2,2,4-三甲基-1,3戊二醇异丁酯:10~20,乙醇:10~35,二丙二醇丁醚:1~3,二氧化硅:1~3,水:70~90。本专利技术与现有技术相比所具有的优点是:在羊毛纤维和维纶纤维内添加增光剂,从而使得羊毛面料光泽度高,使用这种羊毛面料制成的成衣外表美观,手感顺滑。具体实施方式一种外表光泽度高的羊毛面料,包括羊毛纤维和维纶纤维,所述羊毛纤维的规格为细度85s~150s、长度95~115mm;所述维纶纤维 ...
【技术保护点】
一种外表光泽度高的羊毛面料,包括羊毛纤维和维纶纤维,所述羊毛纤维的规格为细度85s~150s、长度95~115mm;所述维纶纤维的规格为3.5~4.5dtex×50 ~ 75mm;其特征在于,羊毛纤维和维纶纤维内含有增光剂,所述羊毛纤维和维纶纤维的重量百分比为:68~85:76~92;所述增光剂包括以下重量百分比的组分:2-甲基-4-异噻唑啉-3-酮: 17 ~32,2-正辛基-4-异噻唑啉-3-酮: 17 ~32,丁二烯‑苯乙烯乳液: 8 ~ 15,纳米二氧化钛: 8 ~ 15,2,2,4‑三甲基‑1,3戊二醇异丁酯: 10 ~ 20,乙醇:10 ~ 35,二丙二醇丁醚:1 ~ 3,二氧化硅:1 ~ 3,水:70 ~ 90。
【技术特征摘要】
1.一种外表光泽度高的羊毛面料,包括羊毛纤维和维纶纤维,所述羊毛纤维的规格为细度85s~150s、长度95~115mm;所述维纶纤维的规格为3.5~4.5dtex×50~75mm;其特征在于,羊毛纤维和维纶纤维内含有增光剂,所述羊毛纤维和维纶纤维的重量百分比为:68~85:76~92;所述增光剂...