The invention discloses a leather dyeing agent, the quality of copies of the following raw materials: 18 to 30 portions of two dibutyl phthalate, lauric acid two butyl tin 9 ~ 14, 7 ~ 12 ethyl acetate, glycerol 7 ~ 12, 3 ~ 9 titanium dioxide, isocyanate 1 ~ 4, 1 ~ 3 triethanolamine copies of trihydroxymethylenepropane three from 1 to 3, 0.1 to 0.3 portions of cyanoacrylate, double cyanoacrylate 0.1 ~ 0.2, 1 ~ 4 antioxidants, defoaming agent 0.8 to 1.5 parts of sodium chloride, 0.5 ~ 1.5, 0.5 ~ 1.5 phr initiator, polyvinyl pyrrolidone 0.1 ~ 0.5, 40 ~ water 70, 3 to 20 portions of dye. The coloring agent has to fill the cracks in the cortex adhesion ability, and has good and quick drying, dyeing and keep the oil content in the cortex, increased after dyeing and oily gloss, conducive to the growth of leather life.
【技术实现步骤摘要】
本专利技术涉及染色剂,具体涉及一种速干粘合皮革染色剂。
技术介绍
皮革使用久了以后容易出现褪色、表皮破损、皲裂等问题,影响外观和使用寿命,直接丢弃十分浪费资源。然而,现有的染料不具备皮质粘合功能,特别是填补皮质裂缝的能力,染料干速也较慢,同时无法兼顾皮质的养护,补充皮革制品的含油含水量的问题,难以增长皮革使用寿命。
技术实现思路
本专利技术的目的在于提供一种速干的,能够粘合皮革制品破损创口的皮革染色剂,针对现有技术,提供一种皮革染色剂。为实现上述目的,本专利技术采取以下技术方案:一种皮革染色剂,其由质量份以下原料组成:邻苯二甲酸二丁酯18~30份,二月桂酸二丁基锡9~14份,醋酸乙酯7~12份,甘油7~12份,二氧化钛3~9份,异氰酸酯1~4份,三乙醇胺1~3份,三羟甲基丙烷1~3份,氰基丙烯酸酯0.1~0.3份,双氰基丙烯酸酯0.1~0.2份,抗氧化剂1~4份,消泡剂0.8~1.5份,氯化钠0.5~1.5份,引发剂0.5~1.5份,聚乙烯吡咯烷酮0.1~0.5份,水40~70份,染料3~20份。本专利技术中,二氧化钛能够增加黏连性,修复皮革表面小创口;增加光泽度,同时能够反射太阳光的直射,减缓皮革的光氧化。本专利技术中,氯化钠能够增加染色剂的流动性。本专利技术中,氰基丙烯酸酯能够粘合皮质,修复裂痕,固化快且无色,外观平整,同时具有良好的耐候性及抗拉强度。本专利技术的有益效果是:1、本专利技术加入二氧化钛,增加黏连性,填补裂缝;增加光泽度,同时能够反射太阳光的直射,减缓皮革的光氧化。2、本专利技术加入氯化钠,提高染色剂的流动性。3、本专利技术加入氰基丙烯酸酯 ...
【技术保护点】
一种皮革染色剂,其特征在于,其由质量份以下原料组成:邻苯二甲酸二丁酯18~30份,二月桂酸二丁基锡9~14份,醋酸乙酯7~12份,甘油7~12份,二氧化钛3~9份,异氰酸酯1~4份,三乙醇胺1~3份,三羟甲基丙烷1~3份,氰基丙烯酸酯0.1~0.3份,抗氧化剂1~4份,消泡剂0.8~1.5份,氯化钠0.5~1.5份,引发剂0.5~1.5份,聚乙烯吡咯烷酮0.1~0.5份,水40~70份,染料3~20份。
【技术特征摘要】
1.一种皮革染色剂,其特征在于,其由质量份以下原料组成:邻苯二甲酸二丁酯18~30份,二月桂酸二丁基锡9~14份,醋酸乙酯7~12份,甘油7~12份,二氧化钛3~9份,异氰酸酯1~4份,三乙醇胺1~3份,...