The invention of the oil additives, polyvinyl acetal resin by 3 5 copies, 8 copies of ethylene glycol 5, glycerol three acetate 5 silicone oil 35 6 copies, 50 copies, 15 copies of morpholine salt 7 oleic acid, 1 acetone isopropanol 1 3 copies, 3 copies, 3 copies of 1 ethanol, petroleum 5 10 copies of sulfonate, glycidyl ether trimethoxysilane 25 30 copies, 8 copies of 5 sodium carbonate, acrylic vinyl pyridine copolymer 3 5, eighteen alkyl amine acetate 1 ~ 2, 10 ~ 15 calcium carbonate, three octyl dimethyl ammonium chloride of 1 ~ 2, fat acid methyl ester sulfonate 1 ~ 2, 1 ~ 2 benzyl naphthalene sulfonic acid sodium salt; water 200 300 parts, all the materials are mixed, in 95 120 DEG C, stirring for 2 3 hours, namely the product; is easy to get raw materials, low cost, green environmental protection, convenient use, advantages good.
【技术实现步骤摘要】
本专利技术属于一种油田化学品,特别涉及一种油田助剂。
技术介绍
油田助剂包括除油剂,清水剂,反相破乳剂,污水澄清剂,破乳剂,钙镁铁离子去除剂。在三次采油过程中,随着聚合物驱和聚表驱增产作业技术在油田的广泛推广,与之伴随而来的采出水处理问题也变得日益尖锐,传统含油污水除油剂一般是无机聚合铝类絮凝剂,这类絮凝剂对一般的含油污水,处理效果较好,但对含有聚合物的污水,则不能达到预期的处理要求。
技术实现思路
:本专利技术的目的在于;提出一种油井助剂。本专利技术的油井助剂,其特征在于:以重量计,由聚乙烯醇缩醛树脂3-5份,乙二醇5-8份,甘油三醋酸酯5-6份,硅油35-50份,吗啉油酸盐7-15份,丙酮1-3份,异丙醇1-3份,乙醇1-3份,石油磺酸盐5-10份,缩水甘油醚氧丙基三甲氧基硅烷25-30份,碳酸钠5-8份,丙烯酸乙烯基吡啶共聚物3-5份,十八烷胺醋酸盐1~2份,碳酸钙10~15份,辛基三甲基氯化铵1~2份,脂肪酸甲酯磺酸钠1~2份,苄基萘磺酸钠1~2份;水200-300份组成,将全部物料混合,在95-120℃下,搅拌反应2-3小时,即得产品。本专利技术与现有技术相比其有益效果是:具有原料易得,成本低,绿色环保,使用方便,效果好的优点。具体实施方式:下面结合实施例对本专利技术作进一步说明,但本专利技术的实施方式不限于此。本专利技术所用的原料可购买获得。实施例本专利技术的油井助剂,其特征在于:以重量计,由聚乙烯醇缩醛树脂3-5份,乙二醇5-8份,甘油三醋酸酯5-6份,硅油35-50份,吗啉油酸盐7-15份,丙酮1-3份,异丙醇1-3份,乙醇1-3份,石油磺酸 ...
【技术保护点】
一种油井助剂,其特征在于:以重量计,由聚乙烯醇缩醛树脂3‑5份,乙二醇5‑8份,甘油三醋酸酯5‑6份,硅油35‑50份,吗啉油酸盐7‑15份,丙酮1‑3份,异丙醇1‑3份,乙醇1‑3份,石油磺酸盐5‑10份,缩水甘油醚氧丙基三甲氧基硅烷25‑30份,碳酸钠5‑8份,丙烯酸乙烯基吡啶共聚物3‑5份,十八烷胺醋酸盐1~2份,碳酸钙10~15份,辛基三甲基氯化铵1~2份,脂肪酸甲酯磺酸钠1~2份,苄基萘磺酸钠1~2份;水200‑300份组成,将全部物料混合,在95‑120℃下,搅拌反应2‑3小时,即得产品。
【技术特征摘要】
1.一种油井助剂,其特征在于:以重量计,由聚乙烯醇缩醛树脂3-5份,乙二醇5-8份,甘油三醋酸酯5-6份,硅油35-50份,吗啉油酸盐7-15份,丙酮1-3份,异丙醇1-3份,乙醇1-3份,石油磺酸盐5-10份,缩水甘油醚氧丙基三甲氧基硅烷25-30份,...